Verify the failure by observing the initial print lines on the build plate. The symptom is confirmed if the extruded filament fails to adhere to the plate surface, curls upward, and accumulates as a molten mass or 'blob' on the exterior metal surface of the hotend assembly rather than remaining on the bed.