Bambu X2D First Layer Failure Due to Hydroscopic Moisture

Check for moisture-induced degradation by observing the extrusion consistency; if the filament appears to bubble, steam, or hiss during the initial purge, it indicates absorbed atmospheric humidity. Confirm this by checking the filament spool's storage conditions or measuring the relative humidity within the AMS or external dry-box, which should remain below 20%.